北京环氧砂浆地坪Beijing epoxy mortar floor ,环氧地坪,环氧树脂地坪,环氧树脂地坪漆,环氧砂浆地坪,环氧自流平,环氧树脂薄涂,【中科京工一八六一一二九三四五四】北京环氧砂浆地坪Beijing epoxy mortar floor工艺好,强度高,经久耐用,美观大方,承接北京环氧砂浆地坪Beijing epoxy mortar floor以及各种耐磨地坪,环氧地坪工程施工项目。 北京环氧砂浆地坪Beijing epoxy mortar floor基面要求 1,水泥基面牢固、结实、不起壳,应杜绝砂浆起壳现象,混凝土层与砂浆找平层较好一起浇筑。若先浇筑混凝土层,则要求砂浆层的厚度不低于40mm,对叉车道的要求则更厚。有关坡度应符合设计要求,允许偏差值为坡度的2%,并且不大于30mm。 2,要求表面不起砂,硬度高,没有水泥粉化现象。新浇筑的水泥砂浆层要充分保养。水泥基面平坦,无凹凸不平、蜂窝麻面、水泥疙瘩,其他涂料、乳胶漆、泡泡糖等残渣。 3,表面干燥,含水率小于6%,无油污,PH值应在6.0-8.0;水泥地坪养护期过后进场施工前5天,基层不能再用水冲洗或被湿润 1, cement base surface, solid, strong, not shell, should put an end to mortar shell phenomenon, with mortar screed-coat best pouring concrete layer. If the concrete layer first, insist on mortar layer thickness is not less than 40 mm, demand for forklift way is more thick. Slope should comply with the design requirements, allowing the deviation value is 2% of the grade, and not more than 30 mm. 2, requires no sand surface, high hardness, no phenomenon of cement powder. To fully maintain new pouring cement mortar layer. Cement base surface is flat, no bumps, uneven, honeycomb pitting surface, cement paint, latex paint, bubble gum and other residue. 3, the surface is dry, the moisture content of less than 6%, no oil, PH value should be in 6.0 to 8.0; Cement floor paint after curing period in 5 days before the construction, basic can't wash with water or wet 中科京工(北京)科技发展有限公司坐落北京中国建筑材料科学研究院22号楼116室内,依托国家建材院的技术优势同时联姻各个高等院校的技术力量为广大的用户提供质量可靠价格实惠的地面建筑材料。公司以技术为核心、视质量为生命、奉用户为上帝,吸引四面八方的客户。 想了解北京环氧砂浆地坪Beijing epoxy mortar floor更多相关信息,可咨询孟经理